SUPERPLAST 300 ®
Characteristics
The steel is developed for the purpose of more qualitative classical qualities of steels – W.Nr. 1.2378, 12311 and 1.2312. Due to the highly clear structure it reaches excellent workability (of about 15% better than by 1.2738), polishability, corrodibility and it increases the quality of surface and mechanical properties of produced injection and pressing parts. Higher heat conductivity SP300® (P) increases the productivity of the tool. Easy weldability and easier repairs and alterations of the mold design.
Suitability
Heat-treated steel to the firmness from 290 to 320 HB is used for big molds for plastics injection and big frames of molds.
Chemical composition of steel Superplast 300®
Steel grade | Chemical composition in % | Hardness in state | |||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
soft-annealed | heat-treated | ||||||||||||
C | Mn | Si | Cr | W | Mo | V | Ni max | Co | P max. | S max. | HB max. | HRC min. | |
Superplast 300® | 0,23 až 0,27 | 1,00 až 1,50 | 0,05 až 0,20 | 1,00 až 2,50 | 0,30 až 0,60 | 1,00 | 0,020 | 0,020 |
Product range
Blocks: deameters up to 950 mm x 2.000 mm
We will deliver any semi-finished products from the above mentioned dimensions. Other dimensions, except for given stock supplies, have to be consulted with us.